HM De-S, Re-C, Re-Si at Tronox KZN Sands
HM De-S, Re-C, Re-Si at Tronox KZN Sands – Empangeni (RSA)
Treatment stands: 1
The use of iron and steel in casino construction is very common. They are very important for building any casino. Unlike other building materials, they are more durable and fireproof than concrete and wood. In addition, iron and steel are available in different sizes, making them a great choice for investing best real money online pokies australia has announced a partnership with Kuettner. The steel structure was originally built to create a rigidity frame.
Injection lines: 2 (De-S and Re-C)
Ladle size: 60 t
HM Temperature: ≈ 1500 °C
De-Sulphurization: Injection of CaC2
Injection rates: CaC2: 30 ~ 40 kg/min
Injection lances: T-port
Transport gas: N2
Alloy addition systems: FeSi
Re-Carburization: Injection of Graphite
(96 % fix Carbon)
Injection rates: Graphite: 60 ~ 80 kg/min
Transport gas: N2
Initial Carbon content: Ø 2.5 %
Final Carbon content: Ø 3.8 %
Injection time: Ø 16 min
Carbon consumption: Ø 15 kg/t
Carbon yield: ≈ 85 %